⬡ Print Profiles HubSlicer Profiles & Filament Database
PrintersDefectsAbout

Blobbing

🔍 Diagnostic Context: "Blobbing" can have several causes, including moisture, temperature, retraction, cooling, material, or machine condition. Check the filament maker's drying guidance and test one change at a time; no single setting is guaranteed to resolve the symptom.

19 reference combinations to compare. They have not been independently tested by this site.

Bambu Lab P1S + Sunlu PETG
240°C / 80°C • 1.2mm retraction • PETG
Bambu Lab P1S + Prusament PETG
250°C / 85°C • 1.0mm retraction • PETG
Creality Ender 3 V3 SE + Sunlu PETG
240°C / 80°C • 1.0mm retraction • PETG
Prusa MK4 + Prusament PETG
250°C / 85°C • 1.0mm retraction • PETG
Creality K1 + Sunlu PETG
250°C / 80°C • 0.8mm retraction • PETG
Bambu Lab A1 Mini + Bambu Lab PETG Basic
255°C / 80°C • 0.8mm retraction • PETG
Bambu Lab X1C + Prusament PETG
250°C / 85°C • 0.8mm retraction • PETG
Prusa XL + Prusament PETG
250°C / 85°C • 1.0mm retraction • PETG
Anycubic Kobra 3 + Sunlu PETG
240°C / 80°C • 1.0mm retraction • PETG
Elegoo Neptune 4 + Sunlu PETG
245°C / 80°C • 0.8mm retraction • PETG
Bambu Lab A1 + Bambu Lab PETG Basic
255°C / 80°C • 0.8mm retraction • PETG
Bambu Lab P1P + Sunlu PETG
240°C / 80°C • 1.2mm retraction • PETG
Bambu Lab X1E + Prusament PETG
250°C / 85°C • 0.8mm retraction • PETG
Bambu Lab A1 Combo + Bambu Lab PETG Basic
255°C / 80°C • 0.8mm retraction • PETG
Bambu Lab X1 Carbon Combo + Prusament PETG
250°C / 85°C • 0.8mm retraction • PETG
Prusa MK4S + Prusament PETG
250°C / 85°C • 1.0mm retraction • PETG
Creality K1 + Prusament PETG
250°C / 85°C • 0.8mm retraction • PETG
Prusa MK4 + Overture PETG
250°C / 85°C • 1.0mm retraction • PETG
Creality Ender 3 V3 SE + eSun PETG
240°C / 80°C • 1.0mm retraction • PETG
All Printers All Filament Brands All Defects